  1. The strain hardening behaviour of an annealed rod during cold rolling is given by  = 700(ε)0.2 MPa, where  is the flow stress at strain ε.
    Flow stress after 50% reduction in area of the annealed rod on cold rolling is approximately
  2. A.
    750 MPa
    B.
    650 MPa
    C.
    609 MPa
    D.
    559 MPa

    View Answer

    Workspace

    Answer : Option B

    Explanation :

    -NA-