- The yield strength of a polycrystalline metal increases from 100 MPa to 145 MPa on decreasing the grain size from 64 μm to 25 μm. The yield strength of this metal (in MPa) having a grain size of 36 μm is
Answer : Option B
Explanation :
-NA-