In process annealing, the hypo-eutectoid steel is
A.
heated from 30° C to 50° C above the upper critical temperature and then cooled in still air
|
B.
heated from 30° C to 50° C above the upper critical temperature and then cooled suddenly in a suitable cooling medium
|
C.
heated from 30° C to 50° C above the upper critical temperature and then cooled slowly in the furnace
|
D.
heated below or close to the lower critical temperature and then cooled slowly
|
Answer : Option D
Explanation :
No answer description available for this question.